F5 (12CrMo19-5), IS AN ALLOY STEEL WITH CHROME THAT HAS ELEVATED MECHANICAL CHARACTERISTICS AND IT IS SUITABLE FOR THE FABRICATION OF PARTS OF INSTALLATIONS THAT REQUIRE AN EXCELLENT RESISTANCE TO EMBRITTLEMENT UNDER PRESSURE AND AT ELEVATED TEMPERATURE (UP TO 600°C).

CORRESPONDENCE TO INTERNATIONAL DESIGNATIONS

QUALITY EUROPE GERMANY FRANCE SPAIN G.B. USA
EN DIN W.n. AFNOR UNE B.S. ASTM
F5 12CrMo19-5 ~ 12CrMo19-5 1,7362 ~ Z15CD5-05 - 625-520 ASTM A182 F5
ASME SA 182

CHEMICAL ANALYSIS

C
max
Mn Si
max
P
max
S
max
Cr Ni
max
Mo Cu
max
0,15 0,30 ÷ 0,60 0,50 0,030 0,030 4,00 ÷ 6,00 0,50 0,44 ÷ 0,65 0,35

CONCENTRATION LIMITS OF THE ELEMENTS THAT ARE NOT INDICATED IN THE TABLE CAN BE DEDUCED IN THE EN 10020 REGULATION.

MECHANICAL CHARACTERISTICS

STEEL NORMALISATION TEMPERATURE 900°C MIN – TEMPERING TEMPERATURE 620°C MIN
SYMBOLIC Re min Rm min  A min Z min Durezza HB
N/mm2 % % max
F5 275 485 20 35 143÷217

USUALLY AVAILABLE EX STOCK

M.T. COLORATION QUALITY HEAT TREATMENT SURFACE DIAMETER (mm)
F5 Normalised and stress relieved rolled / forged turned 20-400
F5 Annealed rolled / forged 20-360

 

 
Download technical sheet
Cookies user preferences
We use cookies to ensure you to get the best experience on our website. If you decline the use of cookies, this website may not function as expected.
Accept all
Decline all
Read more
Analytics
Tools used to analyze the data to measure the effectiveness of a website and to understand how it works.
Google Analytics
Accept
Decline
Advertisement
If you accept, the ads on the page will be adapted to your preferences.
Google Ad
Accept
Decline
Save