F5 (12CrMo19-5)

ASTM A182

Tempéré et Normalisé (+NT) / Recuit (+A)

PROPRIÉTÉS ET UTILISATIONS

F5 (12CrMo19-5), IS AN ALLOY STEEL WITH CHROME THAT HAS ELEVATED MECHANICAL CHARACTERISTICS AND IT IS SUITABLE FOR THE FABRICATION OF PARTS OF INSTALLATIONS THAT REQUIRE AN EXCELLENT RESISTANCE TO EMBRITTLEMENT UNDER PRESSURE AND AT ELEVATED TEMPERATURE (UP TO 600°C).


ASTM A182 F5 (12CrMo19-5)

 

CORRESPONDANCE DÉSIGNATION INTERNATIONALE 

QUALITYEUROPEALLEMAGNEFRANCEESPAGNAG.B.USA
ENDINW.n.AFNORUNEB.S.ASTM
F5 12CrMo19-5 ~12CrMo19-5 1.7362 ~Z15CD5-05 - 625-520 ASTM A182 F5
ASME SA182 F5

 

COMPOSITION CHIMIQUE % (ASTM A182)

C
max
MnSi
max
P
max
S
max
CrNi
max
MoCu
max
0,15 0,30 ÷ 0,60 0,50 0,030 0,030 4,00 ÷ 6,00 0,50 0,44 ÷ 0,65 0,35

LES LIMITES DE CONCENTRATION DES ÉLÉMENTS NON INDIQUÉS DANS LE TABLEAU PEUVENT ÊTRE DÉRIVÉES DE LA NORME EN 10020.

 

CARACTÉRISTIQUES MÉCANIQUES

acier TEMPÉRATURE DE TEMPÉRÉ 900°C MIN – TEMPÉRATURE DE NORMALISATION 620°C MIN
désignation Re min Rm min A min Z min Durezza HB
N/mm2 % % max
F5 275 485 20 35 143÷217

 

NORMALEMENT DISPONIBLE EN STOCK 

Coloration M.T.AciersTraitement thermiqueÉtat de surfaceDiamètre Ø (mm)
F5 Tempéré et Normalisé (+NT)

Ronds laminés

Forgé tourné

25-220
F5 Recuit (+A) Ronds laminés 25-220

 

 
Download technical sheet
Choix utilisateur pour les Cookies
Nous utilisons des cookies afin de vous proposer les meilleurs services possibles. Si vous déclinez l'utilisation de ces cookies, le site web pourrait ne pas fonctionner correctement.
Tout accepter
Tout décliner
En savoir plus
Analytique
Outils utilisés pour analyser les données de navigation et mesurer l'efficacité du site internet afin de comprendre son fonctionnement.
Google Analytics
Accepter
Décliner
Publicité
Si vous acceptez, les annonces présentes sur la page seront adaptées à vos préférences.
Publicité Google
Accepter
Décliner
Sauvegarder