CORRESPONDENCE TO INTERNATIONAL DESIGNATIONS

QUALITYEUROPEGERMANYFRANCESPAING.B.USA
ENDINW.n.AFNORUNEB.S.ASTM
F9 X12CrMo9-1 12CrMo9-1 1.7386 - - - ASTM A182 F9
ASME SA 182

CHEMICAL ANALYSIS

C
max
MnSiP
max
S
max
CrNiMoCu
max
0,15 0,30 ÷ 0,60 0,50 ÷ 1,00 0,030 0,030 8,00 ÷ 10,00 - 0,90 ÷ 1,10 0,35

CONCENTRATION LIMITS OF THE ELEMENTS THAT ARE NOT INDICATED IN THE TABLE CAN BE DEDUCED IN THE EN 10020 REGULATION.

MECHANICAL CHARACTERISTICS

STEEL NORMALISATION TEMPERATURE 900°C MIN – TEMPERING TEMPERATURE 620°C MIN
SYMBOLIC Re min Rm min A min Z min Durezza HB
N/mm2 % % max
F9 380 585 20 40 179÷217

USUALLY AVAILABLE EX STOCK

M.T. COLORATIONQUALITYHEAT TREATMENTSURFACEDIAMETER (mm)
F9 Normalised and stress relieved rolled / forged turned 25-400
F9 Annealed

rolled 

billet

25-380
60-140

 

 
Download technical sheet
Cookies user preferences
We use cookies to ensure you to get the best experience on our website. If you decline the use of cookies, this website may not function as expected.
Accept all
Decline all
Read more
Analytics
Tools used to analyze the data to measure the effectiveness of a website and to understand how it works.
Google Analytics
Accept
Decline
Advertisement
If you accept, the ads on the page will be adapted to your preferences.
Google Ad
Accept
Decline
Save