F22 cl.3 (102CrMo9-10), IS THE MOST COMMONLY USED FOR THE APPLICATIONS WHERE IT IS REQUIRED A GOOD RESISTANCE TO CREEP UP TO 600°C, FOR EXAMPLE IN THERMAL AND NUCLEAR POWER PLANTS AND FOR ROTORS OR PIPINGS THAT TRANSPORT HOT FLUIDS UNDER PRESSURE.

CORRESPONDENCE TO INTERNATIONAL DESIGNATIONS

QUALITY EUROPE GERMANY FRANCE SPAIN G.B. USA
EN DIN W.n. AFNOR UNE B.S. ASTM
F22 cl.3 10CrMo9-10 EN 10222-2 ~ 10CrMo9-10 1,7380 ~ 12CD9-10 F2632 622-515 ASTM A182 F22
ASME SA 182

CHEMICAL ANALYSIS

C Mn Si
max
P
max
S
max
Cr Mo
0,05 ÷ 0,15 0,30 ÷ 0,60 0,50 0,040 0,040 2,00 ÷ 2,50 0,87 ÷ 1,13

CONCENTRATION LIMITS OF THE ELEMENTS THAT ARE NOT INDICATED IN THE TABLE CAN BE DEDUCED IN THE EN 10020 REGULATION.

MECHANICAL CHARACTERISTICS

STEEL NORMALISATION TEMPERATURE 900°C MIN – TEMPERING TEMPERATURE 620°C MIN
SYMBOLIC Re min Rm min  A min Z min Durezza HB
N/mm2 % % max
F22 310 515 20 30 156÷207

USUALLY AVAILABLE EX STOCK

M.T. COLORATION QUALITY HEAT TREATMENT SURFACE DIAMETER (mm)
F22 cl.3 Normalised and stress relieved rolled / forged turned 40-400
F22 cl.3 Annealed rolled 40-220

 

 
Download technical sheet
Cookies user preferences
We use cookies to ensure you to get the best experience on our website. If you decline the use of cookies, this website may not function as expected.
Accept all
Decline all
Read more
Analytics
Tools used to analyze the data to measure the effectiveness of a website and to understand how it works.
Google Analytics
Accept
Decline
Advertisement
If you accept, the ads on the page will be adapted to your preferences.
Google Ad
Accept
Decline
Save