13CrMo4-5 (1.7335) UN ACCIAIO DOLCE AL CRMO, MOLTO TENACE, CEMENTABILE, SALDABILE E RESISTENTE ALLO SCORRIMENTO A CALDO 550° C. É USATO PER LA FABBRICAZIONE DI TUBI PER BOLLITORI E SURRISCALDATORI O PER IL TRASPORTO DI VAPORE SURRISCALDATO E AD ALTA PRESSIONE. É FACILMENTE LAVORABILE ANCHE ALLO STATO GREZZO DI LAMINAZIONE O NORMALIZZATO.
CORRISPONDENZA DESIGNAZIONI INTERNAZIONALI
QUALITÀ | EUROPA | GERMANIA | FRANCIA | SPAGNA | G.B. | USA | |
---|---|---|---|---|---|---|---|
EN | DIN | W.n. | AFNOR | UNE | B.S. | ASTM | |
13CrMo4-5 EN 10222-2 |
13CrMo4-5 | 13CrMo4-4 | 1.7335 | ~ 10CD6 | ~F2631 | ~621 | ~F11 |
ANALISI CHIMICA
C | Mn | Si | P max |
S max |
Cr | Mo | Cu max |
N max |
---|---|---|---|---|---|---|---|---|
0,10 ÷ 0,15 | 0,40 ÷ 0,60 | 0,15 ÷ 0,35 | 0,015 | 0,010 | 0,70 ÷ 1,10 | 0,40 ÷ 0,50 | 0,20 | 0,012 |
I LIMITI DI CONCENTRAZIONE DEGLI ELEMENTI NON INDICATI IN TABELLA SONO DESUMIBILI DALLA NORMA EN 10020.
CARATTERISTICHE MECCANICHE
ACCIAIO | TEMPERATURA DI NORMALIZZAZIONE 900°C MIN - TEMPERATURA DI RINVENIMENTO 620°C MIN | |||||
SIMBOLICA | Re min | Rm | A min | Z min | Durezza HB | |
N/mm2 | % | % | max | |||
13CrMo4-5 | 462 | 440 ÷ 590 | 22 | 30 | - |
NORMALMENTE DISPONIBILE A MAGAZZINO
COLORAZIONE M.T. | QUALITÀ | TRATTAMENTO TERMICO | STATO SUPERFICIALE | DIAMETRO (mm) |
---|---|---|---|---|
13CrMo4-5 | Ricotto | laminato | 60-220 |
Scarica la scheda tecnica |